Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 6.04 MPa | 876 psi | 257°F, 70 hr in IRM 903 Oil; ASTM D471 |
ExxonMobil Geolast® 701-80W183 Thermoplastic Elastomer A soft, black, oil resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good hot air and hot oil resistance for use in a wide range of applic.. |