Polymer Property : Tensile Strength at Break = 580000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 4000 MPa
580000 psi
ASTM D3379-77
SGL Carbon Group SIGRAFIL C® C30 T050 EPY Continuous Tow Carbon Fiber with 50k filaments, Epoxy Sizing
SIGRAFIL C as continuous tow is ideal for waving, prepregging, filament winding, Carbon Fiber Reinforced Plastics (CFRP) components, advanced composites, multi-axial production, unidirectional tapes..