Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 578 MPa | >= 83800 psi | 82 lb. Minimum Tensile Load 0.0353 in. Diameter |
Shakespeare S-3 Economy Nylon Copolymer Fishing Line, 70 lb Information provided by Shakespeare Company. |