Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 0.393 MPa | 57.0 psi | |
Abatron MasterMold 12-8 Flexible Mold Making Compound Master mold 12-8 is a pourable version of MasterMold 12-3 for creating a mold by pouring it into, or around, the model.Processing: Part A Resin: Clear, pourable viscous liquid, 8.7 lbs/galPart B Con.. |