Polymer Property : Tensile Strength at Break = 561 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 561 MPa
>= 81400 psi
234 lb. Minimum Tensile Load 0.0605 in. Diameter
Shakespeare S-3 Economy Nylon Copolymer Fishing Line, 200 lb
Information provided by Shakespeare Company.
Tensile Strength at Break 561 MPa
81300 psi
2.3 lb. load and 0.006 in. diameter
Shakespeare WonderThread® M-7 diameter 0.006" Polyester Industrial Sewing Thread
Applications: Specialty industrial sewing applications demanding polyester for: 1) Certifications that sewn goods are 100% polyester Chemical Resistance-polyester withstands low Ph, acidic enviro..