Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 56.21 MPa | 8153 psi | UNI EN ISO 527-1(97) and UNI EN ISO 527-2(97) |
CRP Technology Windform® GT Polyamide Glass Composite Processed by selective laser sintering (SLS). Windform® GT is a deep and dark black composite material based on polyamide fiber glass. After hand finishing, the color becomes shining and brighter... |