Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 554 MPa | >= 80400 psi | 96 lb. Minimum Tensile Load 0.039 in. Diameter |
Shakespeare FN-29 Freshwater Nylon Copolymer Fishing Line, 80 lb Excellent castability and strength. Economic.Information provided by Shakespeare Company. |