Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | >= 548 MPa | >= 79500 psi | 17 lb. Minimum Tensile Load 0.0165 in. Diameter |
Shakespeare NX-811 Economy Nylon Copolymer Fishing Line, 17 lb Information provided by Shakespeare Company. |