Polymer Property : Tensile Strength at Break = 542 psi
Polymer Property :
Tensile Strength at Break =
542 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
3.74
MPa
542
psi
ISO R 527
Stir SpA E 2055 (PVC)
Application: Extrusion tubular gasketInformation provided by STIR SpA