Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 36.8 MPa | 5340 psi | ISO 527-1,2 |
Nanocyl PLASTICYL™ PP2001 Polypropylene with 3.2 wt% Multi-Wall Carbon Nanotubes PLASTICYL™ is a family of Multi-Wall Carbon Nanotube (MWNT) thermoplastic concentrates for applications requiring superior electrical conductivity and electrostatic discharge (ESD) properties. PLA.. |
|||
Tensile Strength at Break | 36.8 MPa | 5340 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP 246 Toughened Polystyrene Characteristics Excellent clarity Very high toughness Deep drawability Improved thermal stabilityProcessing Extrusion ThermoformingApplications Thermoformed clear and deep draw products Rectangu.. |
|||
Tensile Strength at Break | 36.8 MPa | 5340 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP 6450 High Heat Polystyrene Characteristics High impact and modulus Very good flow properties High heat resistance & strength Available in any dark colorProcessing Injection moldingApplications Instrument enclosures Automo.. |
|||
Tensile Strength at Break | 36.8 MPa | 5340 psi | ASTM D638 |
Total HDPE 46060 UV High Density Polyethylene - Large Part Blow Molding Resin Polyethylene: High molecular weight, high density large part blow molding resin.Characteristics:Good melt strengthGood impact and creep resistanceExcellent stress cracking resistanceExcellent stack.. |
|||
Tensile Strength at Break | 36.8 MPa | 5340 psi | ASTM D3759 |
3M 2552/Silver Damping Foils General purpose vibration dampingInformation provided by 3M |
|||
Tensile Strength at Break | 36.8 MPa | 5340 psi | 50 mm/min; ASTM D638 |
Supreme Petrochem SP EXP 31 Toughened Polystyrene Characteristics Very high clarity & gloss High dart impact strength & good stiffness Good crease retention Good heat resistance High yield compared to PVC, APET Processing Extrusion Vacuum form.. |