Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 3.59 MPa
520 psi
ASTM D412
Teknor Apex Telcar® TL-2717B Thermoplastic Elastomer
Uses: Consumer Applications; Flexible Grips; General Purpose; Grommets; Industrial Soft; Sporting Goods; Toys; Weatherstripping Forms: Pellets Processing Method: Extrusion; Injection Molding Inject..
Tensile Strength at Break 3.59 MPa
520 psi
ASTM D412
Teknor Apex Telcar® TL-88-N873C BLK 111 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Strength at Break 3.59 MPa
520 psi
(20 in/min), Molded Properties; ASTM D638
ExxonMobil Escorene™ UL 15028CC Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 15028CC is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agent..
Tensile Strength at Break 3.59 MPa
520 psi
(20 in/min), Molded Properties; ASTM D638
ExxonMobil Escorene™ UL 15028EM1 Ethylene Vinyl Acetate Copolymer (European Grade)
Product Description: UL 15028EM1 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: Yes Free Flowing Agen..
Tensile Strength at Break 3.59 MPa
520 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8211-45 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..