Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 455 - 505 MPa | 66000 - 73300 psi | 1029 Cold Rolled Steel butt joint. |
Lucas-Milhaupt BRAZE 505 Carbide Brazing Alloy Applications: Braze 505 readily wets nickel and iron base alloys. It is recommended for joining 300 Series stainless steel and will retard interface corrosion in most exposures for which the base m.. |