Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 3.463 MPa | 502.2 psi | 257°F, 70 hr in IRM 903 Oil; ASTM D471 |
ExxonMobil Santoprene® 211-64 Thermoplastic Elastomer
(discontinued **) A soft, colorable, versatile thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in a wide ra.. |