Polymer Property : Tensile Strength at Break = 50000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 276 - 345 MPa
40000 - 50000 psi
Brass butt joint
Lucas-Milhaupt BRAZE 450 Silver Based Cadmium Free Filler Metal
Characteristics:Braze 450 is an intermediate temperature cadmium free silver brazing filler metal with sufficient melting range (145EF) to properly braze joints with the range of fits encountered in..
Tensile Strength at Break 241 - 345 MPa
35000 - 50000 psi
Brass butt joint
Lucas-Milhaupt BRAZE 541 Silver Based Cadmium Free Filler Metal
Characteristics:Braze 541 is an intermediate temperature silver brazing alloy with a rather long, 235EF (130EC) melting range. It has a tendency to liquate (i.e. separate into low and high melting ..
Tensile Strength at Break 276 - 345 MPa
40000 - 50000 psi
Nickel-Silver butt joint
Lucas-Milhaupt BRAZE 700 (Medium) Silver Based Cadmium Free Filler Metal
Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel..
Tensile Strength at Break 241 - 345 MPa
35000 - 50000 psi
Brass butt joint
Lucas-Milhaupt BRAZE 716 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic comp..
Tensile Strength at Break 241 - 345 MPa
35000 - 50000 psi
Brass butt joint
Lucas-Milhaupt BRAZE 716 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal
Characteristics: Braze 716 is a nickel modified silver copper eutectic filler metal. The addition of nickel renders this alloy somewhat more sluggish in flow characteristics than the eutectic comp..
Tensile Strength at Break 241 - 345 MPa
35000 - 50000 psi
Brass butt joint
Lucas-Milhaupt BRAZE 720 Silver Based Cadmium Free Filler Metal
Characteristics:Brazing 720 is the silver-copper eutectic composition and in melting it acts like a metallic element, i.e. it melts completely at a single temperature, thus it will quickly flow into..
Tensile Strength at Break 241 - 345 MPa
35000 - 50000 psi
Brass butt joint
Lucas-Milhaupt BRAZE 721 (VTG) Grade 1 Silver Based Cadmium Free Filler Metal
Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc..
Tensile Strength at Break 241 - 345 MPa
35000 - 50000 psi
Brass butt joint
Lucas-Milhaupt BRAZE 721 (VTG) Grade 2 Silver Based Cadmium Free Filler Metal
Applications: Braze 721, a VTG version of Braze 720, is designed for all types of moderate temperature vacuum systems and particularly where maximum precautions must be taken to insure the presenc..
Tensile Strength at Break 276 - 345 MPa
40000 - 50000 psi
Low Carbon Steel butt joint
Lucas-Milhaupt BRAZE 560
Characteristics:Braze 560 is a low temperature, free-flowing brazing filler metal with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through it..
Tensile Strength at Break 276 - 345 MPa
40000 - 50000 psi
Nickel-Silver butt joint
Lucas-Milhaupt BRAZE 750 (Hard) Silver Based Cadmium Free Filler Metal
Characteristics: This alloy is a intermediate silver brazing filler metals with a slight tendency to liquate (i.e. separate into low and high melting constituents) if heated slowly through their mel..