Polymer Property : Tensile Strength at Break = 500 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 420 - 500 MPa
60900 - 72500 psi
Goodfellow Dural® Aluminum /Copper/Magnesium Alloy
High strength, low weight alloy; in the solution heat-treated and aged condition, mechanical properties are as good as, or better than, low-carbon steel. Limited weldability. Used in aircraft and ae..