Mechanical Properties Metric English Comments
Tensile Strength at Break 5.80 MPa
841 psi
ISO 527
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tensile Strength at Break 5.80 MPa
841 psi
ISO 527
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tensile Strength at Break 5.80 MPa
841 psi
ISO 527
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tensile Strength at Break 5.80 MPa
841 psi
ISO 527
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tensile Strength at Break 5.80 MPa
841 psi
ISO 527
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tensile Strength at Break 5.80 MPa
841 psi
ISO 527
A. Schulman INVISION™ VX-5075UI Soft Touch Polyolefin Thermoplastic
DescriptionInvision™ VX-5075UI is a polyolefin-based thermoplastic of 75 Shore A durometer, which has been formulated for soft touch, mar resistance, low gloss, and excellent weatherability. Appli..
Tensile Strength at Break 5.80 MPa
841 psi
ISO 37
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Extrusion, Black
Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and..
Tensile Strength at Break 5.80 MPa
841 psi
ISO 37
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Extrusion, Natural
Vitaprene® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Vitaprene® compounds permit sophisticated component design and..
Tensile Strength at Break 5.80 MPa
841 psi
ISO 37
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Black
Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu..
Tensile Strength at Break 5.80 MPa
841 psi
ISO 37
ELASTO UK Dryflex® 8009-101 Flame Retardant TPE for Injection Molding, Natural
Dryflex® thermoplastic elastomers combine the performance of most vulcanized rubber with the process properties of thermoplastics. Dryflex® compounds permit sophisticated component design and thu..
Tensile Strength at Break 5.80 MPa
841 psi
ISO 527-1
Barlog Plastics KEBAFLEX E 65.1 TPE-V, Shore A65
TPE-VInformation provided by BARLOG plastics GmbH.
Copyright © lookpolymers.com All Rights Reserved