Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.62 MPa @Temperature 23.0 °C |
815 psi @Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ CL40 Thermoplastic Elastomer (TPE) Versaflex™ CL40 is an easy processing compound designed for use in injection molding applications where water-clarity and excellent colorability are required. - Excellent Clarity - Excellent Colora.. |
|||
Tensile Strength at Break | 5.62 MPa @Time 7200 sec |
815 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7375-9000 TPE Product Description: StarFlex P 7375-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |