Polymer Property : Tensile Strength at Break = 5.47 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 5.47 MPa
793 psi
Longitudinal; ASTM D3759
3M Scotch® 660 Red Cellophane Tape
Scotch® Cellophane Tape 660 is a high performance red film tape featuring a high tack adhesive system and is recommended for splicing, high temperature applications, carton closure and decorative p..