Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 5.40 MPa | 783 psi | After oven air again 168 hrs. @ 150°C; ASTM D412 |
Advanced Elastomer Systems Santoprene® 8281-75 Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic medical grade elastomer. It has USP Class VI Certificate of Compliance for biocompatibility and can be processed using injection molding, extrusion, or other .. |
|||
Tensile Strength at Break | 5.40 MPa | 783 psi | Across Flow; ASTM D412 |
ExxonMobil Santoprene® 121-62M100 Thermoplastic Elastomer A soft, black, UV resistant thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in difficult .. |
|||
Tensile Strength at Break | 5.40 MPa | 783 psi | ISO 37 |
Alliance Polymers Viprene™ G50A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 5.40 MPa | 783 psi | ISO 37 |
Alliance Polymers Viprene™ G50A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 5.40 MPa | 783 psi | ISO 37 |
Alliance Polymers Viprene™ G50D-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Strength at Break | 5.40 MPa | 783 psi | ISO 37 |
Alliance Polymers Viprene™ G50D-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G50D-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |