Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 33.6 MPa | 4870 psi | 67% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Fuel C/E10 for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |