Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 48.9 MPa | 7090 psi | Tensile stress at break. |
Dow Pellethane® 2102-90AR Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-90AR elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced mold release, low compression set, a.. |
|||
Tensile Strength at Break | 48.9 MPa | 7090 psi | 97% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Methyl Ethyl Ketone for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |