Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 48.00 MPa | 6962 psi | |
Indium Corp. Indalloy® 241 95.5Sn/3.8Ag/0.7Cu Lead-Free Solder Alloy Multicore promoted alloy.Information provided by the manufacturer, Indium Corporation. |