Mechanical Properties Metric English Comments
Tensile Strength at Break 479 - 607 MPa
69500 - 88000 psi
18-8 Annealed Stainless Steel butt joint.
Lucas-Milhaupt BRAZE 505 Carbide Brazing Alloy
Applications: Braze 505 readily wets nickel and iron base alloys. It is recommended for joining 300 Series stainless steel and will retard interface corrosion in most exposures for which the base m..