Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 46.4 MPa | 6730 psi | 92% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Acetic Acid (10%) for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 46.4 MPa | 6730 psi | 92% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Water for 500 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 46.4 MPa | 6730 psi | ASTM D412 |
Compuestos Dominicanos Polycom PF-102199 PVC Compound Compuestos Dominicanos' rigid PVC compounds for the extrusion of pipes have excellent processing characteristics and are available in the form of pellets and dry-blend. Also available are compounds.. |