Mechanical Properties Metric English Comments
Tensile Strength at Break 31.63 MPa
4588 psi
ASTM D638
Plastics Group Polifil® M-20 20% Mica-Reinforced Polypropylene
Polifil® M series compounds are homopolymer polypropylene resins reinforced with mica. They combine an improved range of high-stiffness values with low mold shrinkage. These compounds are used in l..