Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 45.1 MPa @Thickness 2.00 mm |
6540 psi @Thickness 0.0787 in |
50mm/min; ASTM D638 |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Tensile Strength at Break | 45.1 MPa | 6540 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Tensile Strength at Break | 45.1 MPa | 6540 psi | 50 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® QP-1010 PC/ABS, Unreinforced FR Information provided by Samsung Cheil Industries. |