Mechanical Properties Metric English Comments
Tensile Strength at Break 44.7 MPa
6480 psi
ASTM D 638
NOVA Chemicals Dylark® 432 High-Heat Styrenic Copolymer
Product Description and Features: Styrenic copolymer with excellent heat resistance and good modulus. Resin designed for use as an additive to promote adhesion and compatibility in compounding of ..