Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 30.1 MPa | 4360 psi | ASTM D638 |
Westlake Plastics Propylux® HS Polypropylene-heat stabilized For Medical Applications Medical grade Propylux HS is made from an FDA approved polypropylene resin. Through a unique heat-stabilizing process, the extruded material is able to withstand higher temperature with less water .. |