Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 434 MPa | 63000 psi | |
Shakespeare WN-50 diameter 0.2 mm Nylon Monofilament 610 Paper Machine Clothing MonofilamentDimensionally stableNylon 6,10Moderate ModulusLow moisture regainModerate shrinkage Information provided by Shakespeare Company. |
|||
Tensile Strength at Break | 434 MPa | 63000 psi | |
Shakespeare WN-50 diameter 0.4 mm Nylon Monofilament 610 Paper Machine Clothing MonofilamentDimensionally stableNylon 6,10Moderate ModulusLow moisture regainModerate shrinkage Information provided by Shakespeare Company. |