Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.96 MPa | 429 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9065 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9000 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9000 Series of compoun.. |