Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 295.2 MPa | 42810 psi | Property derived with 10 Ply Laminate, hand Lay-up, Style 181 Glass Fabric, 55% Glass Content.; ASTM D638 |
Fibre Glast ProSet 125R / 229H Epoxy
(discontinued **) Information provided by Fibre Glast Developments Corporation. |