Mechanical Properties Metric English Comments
Tensile Strength at Break 29.2 MPa
4230 psi
ASTM D638
Westlake Plastics Propylux® 290 Polypropylene, Heat Stabilized
Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux 290 is produced from a FDA approved homopolymer res..
Tensile Strength at Break 29.2 MPa
4230 psi
ASTM D638
Westlake Plastics Propylux® HS2 Polypropylene for Medical Applications, Heat Stabilized
Through process improvement and advanced engineering, Westlake Plastics introduces the next generation of heat-stabilized polypropylene. Propylux HS2 is produced from a FDA and USP Class VI approve..
Tensile Strength at Break 29.2 MPa
4230 psi
ASTM D3756
3M 203 Masking Tape
3M™ Masking Tape 203 is a general purpose masking tape that can be used for holding, bundling, sealing and a vast number of other jobs where a pressure- sensitive tape is needed.Information provide..