Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 28.6 MPa | 4150 psi | chs 2.0 in/min; ASTM D882 |
Diamond Polymers MS-170 Styrene Methyl Methacrylate Terpolymer Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |