Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 28.3 MPa | 4110 psi | ASTM D882 |
Westlake Plastics PMP Film Made from TPX® Polymethylpentene Resin Lowest specific gravity of any known thermoplastic. Exceptional electrical properties. Good chemical resistance. High heat resistance. Excellent acoustical properties. Transparency. FDA compli.. |
|||
Tensile Strength at Break | 28.3 MPa | 4110 psi | ASTM D3759 |
3M Scotch® 265 Fine Line Tape Scotch® Fine Line Tape 265 is a high-performance film backed tape designed for in-mold fine line masking where sharp, clean, gel-coat color separation lines are desired.Information provided by 3M |