Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 40.9 MPa | 5930 psi | 81% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Isopropanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |
|||
Tensile Strength at Break | 40.9 MPa | 5930 psi | ASTM D3759 |