Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 40.21 MPa | 5832 psi | |
Taiwan PU Corporation TPUI-E95 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |