Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.76 MPa | 690 psi | ASTM D638 |
ExxonMobil OPTEMA™ TC 130 Molding, extrusion and compounding resin
(discontinued **) OPTEMA TC 130 is an ethylene methyl acrylate copolymer, which can be used in specialty applications such as a carrier for color and additive master batches, a compatibilizer in polymer compounds and.. |