Polymer Property : Tensile Strength at Break = 4.60 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 4.60 MPa

@Temperature 280 °C
667 psi

@Temperature 536 °F
ASTM D1708
Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA)
Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res..
Tensile Strength at Break 4.60 MPa
667 psi
ISO R 527
Stir SpA IN 3080 CZ (PVC)
Application: Extrusion fillerInformation provided by STIR SpA
Tensile Strength at Break 4.60 MPa
667 psi
ASTM D412
Sumitomo Chemical ESPOLEX® 3675 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Tensile Strength at Break 4.60 MPa
667 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8211-55 Thermoplastic Elastomer
A soft, colorable, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. This material combines good physical properties and chemical resistance for use in dif..
Tensile Strength at Break 4.60 MPa
667 psi
Across Flow; ASTM D412
ExxonMobil Santoprene® 8281-55MED Thermoplastic Elastomer
A soft, colorable, specialty, non-hygroscopic thermoplastic vulcanizate (TPV) in the thermoplastic elastomer (TPE) family. USP Class VI Certificates of Compliance exist for representative samples of..