Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.481 MPa | 649.9 psi | In Air, Across Flow, Change in tensile strength after 24 hours at 275°F; ASTM D573 |
Teknor Apex Uniprene® UN-7100-55 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |