Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 4.31 MPa @Time 7200 sec |
625 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7350-1000 TPE Product Description: StarFlex P 7350-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tensile Strength at Break | 4.31 MPa @Time 7200 sec |
625 psi @Time 2.00 hour |
Die C; ASTM D414 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 55-9000 TPE Product Description: StarGrip GP 55-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubbery.. |
|||
Tensile Strength at Break | 4.31 MPa | 625 psi | ASTM D412 |
Teknor Apex Monprene® MP 1249D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.31 MPa | 625 psi | ASTM D412 |
Teknor Apex Monprene® MP-1709A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 4.31 MPa | 625 psi | ASTM D412 |
Teknor Apex Telcar® TL-1120E Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |