Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.72 MPa | 395 psi | ASTM D3759 |
3M Scotch® 8886 Stretchable Tape Scotch® Stretchable Tape is a high performance transparent stretchable tape, designed to contain A- and B- pallets for internal and external shipping purposes.Information provided by 3M |