Mechanical Properties Metric English Comments
Tensile Strength at Break 0.275 MPa
39.9 psi
Dynamic, 1 in.<sup>2</sup> (6.45 cm<sup>2</sup>) overlap Jaw Speed 0.5 in./min (12.7 mm/min.); ASTM D-897
3M 4466B Double Coated Polyethylene Foam Tape
3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in..
Tensile Strength at Break 0.275 MPa
39.9 psi
Dynamic, 1 in.<sup>2</sup> (6.45 cm<sup>2</sup>) overlap Jaw Speed 0.5 in./min (12.7 mm/min.); ASTM D-897
3M 4466W Double Coated Polyethylene Foam Tape
3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in..
Tensile Strength at Break 0.275 MPa
39.9 psi
Dynamic, 1 in.<sup>2</sup> (6.45 cm<sup>2</sup>) overlap Jaw Speed 0.5 in./min (12.7 mm/min.); ASTM D-897
3M 4496B Double Coated Polyethylene Foam Tape
3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in..
Tensile Strength at Break 0.275 MPa
39.9 psi
Dynamic, 1 in.<sup>2</sup> (6.45 cm<sup>2</sup>) overlap Jaw Speed 0.5 in./min (12.7 mm/min.); ASTM D-897
3M 4496W Double Coated Polyethylene Foam Tape
3M™ Double Coated Polyethylene Foam Tapes 4462W, 4462B, 4466W and 4466B combine a conformable closed cell foam with a rubber adhesive that provides high initial adhesion to a variety of surfaces in..
Tensile Strength at Break 0.275 MPa
39.9 psi
T Block, 1 in<sup>2</sup> (6.45 cm<sup>2</sup>) Jaw Speed 2 in/min (50 mm/min)
3M 4026 Double Coated Urethane Foam Tape
3M™ Double Coated Urethane Foam Tapes are conformable foams that offer high shear strength and are available with either a high temperature holding acrylic adhesive system or a rubber adhesive syst..