Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 2.62 MPa | 380 psi | ASTM D412 |
Teknor Apex Telcar® TL-2507B Thermoplastic Elastomer Uses: Consumer Applications; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderat.. |
|||
Tensile Strength at Break | 2.62 MPa | 380 psi | ASTM D412 |
Aearo E-A-R Specialty Composites VersaDamp™ V-2325 TPE VersaDamp TPEs are olefinic dynamic vulcanizates. The VersaDamp 2000 series materials provide predictable damping performance throughout a broad range of temperatures. They can be injection molded.. |