Polymer Property : Tensile Strength at Break = 37100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 256 MPa
37100 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP Lubricomp UCL36AS PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UCL36AS is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.This data ..
Tensile Strength at Break 256 MPa
37100 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP LUBRICOMP UCL36ASP PPA (Europe-Africa-Middle East)
LNP* LUBRICOMP* UCL36ASP is a compound based on Polyphthalamide resin containing Carbon Fiber, PTFE. Added features include; Internally Lubricated, Electrically Conductive, Heat Stabilized.
Tensile Strength at Break 256 MPa
37100 psi
5 mm/min; ISO 527
SABIC Innovative Plastics LNP THERMOCOMP LC008EXP PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LC008EXP is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include Electrically Conductive, Easy Molding.
Tensile Strength at Break 256 MPa
37100 psi
ISO 527
SABIC Innovative Plastics LNP VERTON RV00AES PA 66
LNP VERTON* RV00AES is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, Structural.
Tensile Strength at Break 256 MPa
37100 psi
ISO 527
SABIC Innovative Plastics LNP VERTON RX06422 PA 66
LNP VERTON* RX06422 is a compound based on Nylon 66 resin containing 50% Long Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized, UV Stabilized, Structural.