Mechanical Properties Metric English Comments
Tensile Strength at Break 25.376 MPa

@Temperature 100 °C,
Time 252000 sec
3680.5 psi

@Temperature 212 °F,
Time 70.0 hour
After Dry Heat Aging; ASTM D865
Seals Eastern 7168 Nitrile Rubber
Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc.