Polymer Property : Tensile Strength at Break = 3490 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 24.1 MPa
3490 psi
ASTM D3756
3M 301+ Performance Yellow Masking Tape
3M™ Performance Yellow Masking Tape 301+ is an industrial strength yellow colored smooth crepe paper masking tape for paint masking, holding, bundling, and identifying applications.Information prov..