Polymer Property : Tensile Strength at Break = 348 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 1.80 - 2.40 MPa
261 - 348 psi
ASTM D415
Proto3000 Objet TangoBlack FullCure970 Rubber-like Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..