Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 34.8 MPa | 5050 psi | ASTM D638 |
Niche Polymer PPHT20BK Homopolymer PP, 20% Talc Fiber Filled Information provided by Niche Polymer |
|||
Tensile Strength at Break | 34.8 MPa | 5050 psi | ASTM D638 |
Sterigenics Raprex® R-100 Branched High Density Polyethylene Applications: ExtrusionRAPREX® R-100 is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched struct.. |
|||
Tensile Strength at Break | 34.8 MPa | 5050 psi | 69% Ret. |
UBE UBESTA® 3030U Nylon 12 (After Methanol for 1000 hours) Description: UBESTA has a strong resistance to chemicals. Under normal conditions, it is not significantly affected by alkalis, alcohols, ethers, ketones, hydrocarbons, lubricating oils, gasoline, c.. |