Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 34.32 MPa | 4978 psi | |
Taiwan PU Corporation TPU-BH95 Hydrolysis Resistance, Blow Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow MoldingInformation provided by Taiwan PU Corporation. |
|||
Tensile Strength at Break | 34.32 MPa | 4978 psi | |
Taiwan PU Corporation TPU-E90 General Grade, Extrusion Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |
|||
Tensile Strength at Break | 34.32 MPa | 4978 psi | |
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation. |