Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 23.2 MPa | 3360 psi | 510 mm/min; ASTM D412A |
PolyOne Elastamax™ XL 0131-59 Styrene Butadiene Block Copolymer (SBC) A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in acco.. |
|||
Tensile Strength at Break | 23.2 MPa | 3360 psi | |
Taiwan PU Corporation UR60 Polyester Urethane Rubber UR60 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |